MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Methylon 75202 Metal Coating Resin
Categories: Polymer; Thermoplastic

Material Notes: DESCRIPTION: Methylon 75202 is a metal coating resin produced by the reaction of a bisphenol epichlorohydrin type epoxy resin with a xylene-formaldehyde condensation polymer in a mixture of xylol, diacetone alcohol and butyl cellosolve.

APPLICATION: Methylon 75202 should be used where color and flexibility are important as in appliance primers.

USES:

  • Linings for drums, cans and pails.
  • Finishes for appliances.
  • Industrial coating requiring light color, chemical resistance and flexibility.
  • Primers needing chemical resistance properties.

FEATURES:

  • Light color and excellent flexibility.
  • Outstanding resistance to chemicals, solvents, acids, alkalis, and soap solutions.
  • Compatible with epoxies, polyvinyl butyral, short and medium oil alkyds, urea and melamine formaldehyde resins.
  • Cured films have excellent adhesion, heat resistance and mar-resistance.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccDCT 5075
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 13G-H; DCT 4075A
 
Descriptive Properties
G&H ViscosityZ3DCT 4003A
Non Volatile (%)65125°C, 2.5 g, 45 min; DCT 4064A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman Araldite GY 6010 Bisphenol A Epoxy Liquid Resin
Overview of materials for Epoxy/Carbon Fiber Composite

PSUMIT171 / 193976

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.