MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wingate Alloys Winco 34 General Purpose Corrosion and Abrasion Resistant Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Winco 34 is a general purpose, high tensile Stainless Steel with corrosion and abrasion resistance and physical properties equal to or superior to those of typical 304, 18-8 Stainless Steel.
    Advantages:
  • Free machining and non-magnetic.
  • Corrosion Resistant – resists pitting and oxidation at elevated temperatures.
  • Corrosion resistance is not affected by normal brazing, welding and stress relieving.
  • Heat Resistant – acceptable high strength performance in applications up to 1600°F.
  • Resists warping due to temperature changes.
  • Abrasion Resistant – increased Nickel and Chromium aids in wearabilty superior to that of standard grades of Stainless Steel.
  • All bars are delivered machine straightened and stress relieved.
  • Precision tolerances on Turned, Ground and Polished shafting.
  • Exhibits minimal carbide precipitation during welding.
Applications: Arbors, hoppers spindles, shafts, chutes, pins, troughs, cute liners and scraper blades.

Information from Wingate Alloys Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
303 Stainless Steel, annealed
304 Stainless Steel
302 Stainless Steel, annealed strip
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC)
Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel

NWINGA28 / 122092

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.