MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Toray TOYOLAC™ ABS Resin TP50-X03 ABS Polymer
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Durable anti-static, heat resistant, high impact, PC+ABS.

General Toyolac™ Notes: TOYOLAC™ ABS is a versatile thermoplastic consisting of acrylonitrile, butadiene, and styrene and it has unique set of properties combining strength, lightness, and aesthetics. TOYOLAC™ is widely used in both industrial and household goods due to its excellent mechanical, chemical, electrical properties, and superior processability.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Melt Flow 17 g/10 min
@Load 9.99 kg,
Temperature 220 °C
17 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R  116
@Temperature 23.0 °C
116
@Temperature 73.4 °F
50% RH; ASTM D785
 116
@Temperature 23.0 °C
116
@Temperature 73.4 °F
ISO 2039-2
Tensile Strength 55.0 MPa7980 psiASTM D638
 60.0 MPa
@Temperature 23.0 °C
8700 psi
@Temperature 73.4 °F
ISO 527-1,2
Elongation at Break 10 %10 %ASTM D638
 50 %
@Temperature 23.0 °C
50 %
@Temperature 73.4 °F
ISO 527-1,2
Flexural Strength 83.0 MPa12000 psiASTM D790
 91.0 MPa
@Temperature 23.0 °C
13200 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 2.25 GPa326 ksiASTM D790
 2.36 GPa
@Temperature 23.0 °C
342 ksi
@Temperature 73.4 °F
50% RH; ISO 178
Izod Impact, Notched 1.37 J/cm
@Thickness 12.7 mm,
Temperature 23.0 °C
2.57 ft-lb/in
@Thickness 0.500 in,
Temperature 73.4 °F
V-notched; ASTM D256
Charpy Impact, Notched 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
V-Notched; ISO 179
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 3.00e+13 ohm
@Temperature 23.0 °C,
Time 86400 sec
3.00e+13 ohm
@Temperature 73.4 °F,
Time 24.0 hour
50% RH; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 103 °C217 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9200 / 248889

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.