Product Description: A soft, black SEBS based thermoplastic elastomer (TPE) compound designed for use in medical applications. The Bondable to: PP, EVA, PE Availability: Africa & Middle East; Asia Pacific; Europe; North America Features: Block Copolymer; Bondability; Soft Uses: Medical/Healthcare Applications Agency Ratings: USP Class VI RoHS Compliance: RoHS Compliant Appearance: Black Forms: Pellets Processing Method: Injection Molding; ExtrusionInformation provided by Elastron |