MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Elexar® E-8712R Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Elexar EL-8712R is a flame retardant thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Elexar EL-8712R is a medium durometer grade that is RoHS compliant and suitable for both injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Flame Retardant; General Purpose; Good Colorability; Good Flexibility; Halogenated; Heat Aging Resistant; High Density; High Elasticity; High Elongation; High Specific Gravity; High Tensile Strength; Low Flow; Medium Hardness

Uses: Appliance Wire Insulation; Appliance Wire Jacketing. Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
Melt Flow 3.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 71ASTM D2240
Tensile Strength at Break 2000 psiDie C, 20 in/min, 0.02 in; ASTM D412
 1840 psi
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D573
 2180 psi
@Treatment Temp. 108 °C,
Time 605000 sec
In Air; ASTM D573
Tensile Stress at Strain 360 psi
@Strain 100 %,
Thickness 0.508 mm
Die C, 20 in/min; ASTM D412
 530 psi
@Strain 300 %,
Thickness 0.508 mm
Die C, 20 in/min; ASTM D412
Elongation at Break 680 %Die C, 20 in/min, 0.02 in; ASTM D412
 673 %
@Treatment Temp. 108 °C,
Time 605000 sec
In Air; ASTM D471
 700 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D471
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.60e+15 ohm-cmASTM D257
Dielectric Constant 2.1
@Frequency 1000 Hz
ASTM D150
 2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 660 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 221 °FContinuous; ASTM D794
Brittleness Temperature -76.0 °FASTM D746
Flammability, UL94 V-2
@Thickness 3.05 mm
ALL
Oxygen Index 20 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 430 - 445 °FMelt, Injection
Rear Barrel Temperature 390 - 420 °FInjection
Middle Barrel Temperature 415 - 430 °FInjection
Front Barrel Temperature 430 - 440 °FInjection
Nozzle Temperature 430 - 445 °FInjection
Zone 1 380 - 410 °FExtrusion
Zone 2 390 - 420 °FExtrusion
Zone 3 415 - 430 °FExtrusion
Zone 4 415 - 430 °FExtrusion
Zone 5 430 - 440 °FExtrusion
Die Temperature 430 - 445 °FExtrusion
Mold Temperature 77.0 - 150 °FInjection
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 2299 X 80218 Polyetheretherketone (PEEK), PTFE Lubricated
Polyplastics TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC)
Overview of materials for Epoxy Molding Compound
Daikin NEOFLON® AP-231SH PFA
Daikin NEOFLON® AP-230 PFA

PTEKNQ0635 / 237126

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.