MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
UNIPLAS LCA® N66-71G13HSL Black Nylon 66, 13% Glass Fiber, Heat Stabilized, Impact Modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled; Nylon 66, Heat Stabilized; Nylon 66, Impact Grade

Material Notes: Nylon 66 13% Glass Fiber, Heat Stabilized, Lubricated, Impact Modified

Information provided by Uniplas, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Maximum Moisture Content 0.20[%]
Ash 13 %ASTM D5630
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 76.0 MPaASTM D638
Elongation at Break 12 %ASTM D638
Flexural Modulus 3712 MPaASTM D790
Izod Impact, Notched 107 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 255 °CASTM D789-92e1
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 540 - 580 °F
Middle Barrel Temperature 530 - 570 °F
Front Barrel Temperature 520 - 570 °F
Nozzle Temperature 510 - 560 °F
Mold Temperature 150 - 250 °F
Drying Temperature 175 °FDehumidifier
Dry Time 2.00 - 4.00 hourDehumidifier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PUNIPL041 / 306877

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.