MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phon Tech PHOENIX™ 06751 White TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: PHOENIX™ White Thermoplastic Elastomer (TPEs) product family creates diverse features than transparent or translucent materials have. For example, matt finish, silky smooth and dry gripping feels which provide distinguish value to the products. Most important of all, this product family is filler added and hence provide an economical solution for those who are looking for alternatives to reduce cost. This product family is well designed, verified, and fine tuned to meet different customers' requests. Each grade of PHOENIX™ White TPE compounds is the essence of abundant experience, knowledge and sophisticated technology.

Features:

  • Wide range of hardness (Shore 15A ~ 95A)
  • Anti-slip
  • Non-sticky
  • Easy to process and color
  • Overmolding to PP, PE
  • Economy
  • Good resilience
  • Meet FDA requirements
Applications: Screwdriver grip, garden tool grip, knife grip, pen grip, food container seal, car mat, cutting board, sink plug, toothbrush, razor, bicycle handle grip, motorcycle handle grip, scuba diving fins, etc.

Information provided by Phon Tech Industrial Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 - 1.09 g/cc1.03 - 1.09 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 72 - 7872 - 78ASTM D2240
Tensile Strength 3.318 MPa481.2 psiASTM D412
Elongation at Break 434.5 %434.5 %ASTM D412
100% Modulus 2.395 MPa347.4 psiASTM D412
Tear Strength 22.42 kN/m127.9 pliASTM D624 Die C
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPHONT050 / 296392

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.