MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Covestro Bayhytherm® 3146 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Water-reducible, aliphatic, self-crosslinking stoving urethane resin. Binder for waterborne, one-component stoving polyurethane systems

Properties / Applications: Bayhytherm® 3146 is used for the formulation of waterborne, one component baking systems such as waterborne fillers or general purpose industrial coatings. Coating films based on Bayhytherm® 3146 exhibit extraordinary impact strength, adhesion and overcoatability. Bayhytherm® 3146 can also be used as an additive to conventional waterborne stoving systems to improve flexibility, impact strength and adhesion. The product is characterized by a high reactivity, good pigment wetting and thermal stability. Because it is easier to dilute, it also offers advantages with respect to the solids content and filling power of the coating systems at spray viscosity. Typical curing parameters are 30 min at 130 °C. The product exhibits overbaking stability up to 120 min at 190 °C. Slight thermal yellowing may occur depending on the baking temperature and time.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccDIN EN ISO 2811
Volatiles 53 - 55 %53 - 55 %1 g / 1 h / 105 °C; DIN EN ISO 3251
Viscosity 200 - 1200 cP200 - 1200 cPD = 186 s-1; DIN EN ISO 3219/A.3
 
Chemical PropertiesMetricEnglishComments
Acid Value 7.0 - 9.07.0 - 9.0[mg KOH/g]; DIN EN ISO 2114
 
Descriptive Properties
Appearanceyellowish-white, cloudy

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayhydrol® UH 2342 Polyurethane Coating
Covestro Baybond® PU 403 Polyester Urethane Polymer

PCOVEST0205 / 201988

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.