MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
1,3-Propenediol
Categories: Fluid; Solvent

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.053 g/cc
@Temperature 20.0 °C
Viscosity 53.649 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 76.096 g/mol
Vapor Pressure 0.00400 torr
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 59.0 atm
Critical Temperature 385 °C
Critical Density 0.316 g/cc
Critical Molar Volume 241 cm³/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 742.3 J/g
Specific Heat Capacity 1.313 J/g-°C
@Temperature 25.0 °C
Vapor
Melting Point -26.8 °C
Boiling Point 214.5 °C
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter17.2917
Antoine's Vapor Pressure B Parameter3888.84
Antoine's Vapor Pressure C Parameter-123.2
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
Critical Compressibility (Zc)0.26
Dipole moment (p/C.m)1.234E-27
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A1813
Dynamic Viscosity Parameter B406.96
Molar Heat Capacity (298K)99.914 J/mol-K
Molar Heat Capacity of Vapor a Parameter8.2634
Molar Heat Capacity of Vapor b Parameter0.3673
Molar Heat Capacity of Vapor c Parameter-0.000216
Molar Heat Capacity of Vapor d Parameter5.05E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

VORGS296 / 99653

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.