MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Huntsman PE 1008 Film Extrusion Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Homopolymer, and FDA compliant.

Features: Superior strength, good machinability, and heat seal characteristics.

Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, and bundling.

FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170

Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.

Information provided by Huntsman Corporation

Key Words: LDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D1505
Thickness 25.4 microns1.00 mil
Melt Flow 0.80 g/10 min0.80 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5151ASTM D2240
Tensile Strength, Ultimate 14.0 MPa2030 psiASTM D638
Tensile Strength, Yield 10.0 MPa1450 psiASTM D638
Film Elongation at Break, MD 150 %150 %ASTM D882
Film Elongation at Break, TD 500 %500 %ASTM D882
Elongation at Break 650 %650 %ASTM D638
Modulus of Elasticity 0.276 GPa40.0 ksiSecant; ASTM D638
Secant Modulus, MD 0.238 GPa34.5 ksiASTM D882
Secant Modulus, TD 0.276 GPa40.0 ksiASTM D882
Dart Drop 3.54 - 3.94 g/micron90.0 - 100 g/milASTM D1709
Dart Drop Test 90.0 - 100 g0.198 - 0.221 lbASTM D1709
Film Tensile Strength at Break, MD 22.0 MPa3190 psiASTM D882
Film Tensile Strength at Break, TD 21.0 MPa3050 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 99.0 °C210 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 45 %45 %at 45°; ASTM D523
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUO76 / 47785

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.