MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wieland Portadur P2 Casting Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy

Material Notes: Gold casting alloy

Applications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneering

Dental

Key Words: EN ISO 1562
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 15.3 g/cc0.553 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 230230HV5/30; as cast
 230230HV5/30; hardened
Tensile Strength, Yield  600 MPa
@Strain 0.2 %
87000 psi
@Strain 0.2 %
as cast
 600 MPa
@Strain 0.2 %
87000 psi
@Strain 0.2 %
hardened
Elongation at Break 15 %15 %as cast
 15 %15 %hardened
Modulus of Elasticity 98.0 GPa14200 ksi
 
Thermal PropertiesMetricEnglishComments
Melting Point 888 - 932 °C1630 - 1710 °F
Solidus 888 °C1630 °F
Liquidus 932 °C1710 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 699 °C1290 °FPreheating Temp.
Casting Temperature 1080 °C1980 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 12.2 %12.2 %
Gold, Au 71 %71 %
Iridium, Ir 0.10 %0.10 %
Palladium, Pd 1.5 %1.5 %
Platinum, Pt 2.5 %2.5 %
Silver, Ag 12.2 %12.2 %
Zinc, Zn 0.50 %0.50 %
 
Descriptive Properties
Coloryellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wieland Porta Maximum PFM Alloy
Wieland Auropal 1 Casting Alloy
Wieland BioPorta G PFM Alloy
Wieland Porta P6 PFM Alloy
Wieland Porta REFLEX® PFM Alloy

NWIELAN21 / 19823

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.