SABIC® PPcompound 37T1030 is a high flow copolymer with 30% talc, offering an excellent balance between stiffness and impact resistance. It has been specially developed for automotive interior parts such as column cladding and door panels.
SABIC® PPcompound 37T1030 is a designated automotive grade.
IMDS ID: 440839684Information provided by SABIC |