MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lucite International Elvacite® 2010 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Elvacite® 2010 is a medium molecular weight methyl methacrylate polymer. 2010 is excellent for use as a general purpose grade for lacquer coatings, such as barrier topcoats for vinyl. It provides high tensile strength and hardness.

Applications: vinyl topcoats, general purpose grade for lacquers

Information provided by Lucite International

Key Words: Methyl Methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
Particle Size 180 - 200 µm180 - 200 µm
Viscosity Measurement 0.383 - 0.4150.383 - 0.415Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 84000 g/mol84000 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.000.00
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 1919Tukon Hardness
Tensile Strength 72.4 MPa10500 psi
Elongation at Break 3.5 %3.5 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 98.0 °C208 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.50 %0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUCIT9451 / 150165

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.