MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SunChemical Gwent C2000808D1 Silver Backlight Ink  (discontinued **)
Categories: Fluid; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Silver Ink C2000808D1 is a low resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has a dark back color when printed and fired on float side of glass and is fully blendable with high resistance ink C2000808D2. It can be printed onto IR or UV black enamels.

Silver Ink C2000808D1 is a grey ink with a pine smell at a ready to use viscosity suitable for firing on glass to form conductive tracks. The ink should be gently stirred before use avoiding the introduction of air bubbles.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 85 %85 %
Particle Size <= 4.0 µm<= 4.0 µmMain Break; Fineness of Grind
 <= 15 µm<= 15 µm3rd Streak; Fineness of Grind
Viscosity 5000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
5000 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer (PK1.1°)
Storage Temperature <= 25.0 °C<= 77.0 °F
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.0030 ohm0.0030 ohmfired; 12 microns thick
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 °C302 °F
Cure Time 7.98 - 15 min0.133 - 0.25 hour
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
Coverage cm2/g110230 mesh stainless steel screen
Printing Mesh counts/inch180 to 340stainless steel or polyester screens

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WGEM080 / 75933

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.