MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Barlog Plastics KEBAFLEX H / SPC 60 A.01 black SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: TPE-S, Shore A59, black, modified for good adhesion to ABS, PC and PC/ABS blends, among others. Also has good adhesion to PC flame retardant.

Properties: flexible, good haptics, adhesion modified, semi-crystalline, soft

Typical areas of application: Sealing elements, Seals, Spring elements, Handles, Haptic components

Industries: Automotive, Electrical and electronics industry, Household appliances, Industry, Mechanical Engineering, Furniture industry, Sports & Recreation

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 59.059.0DIN ISO 7619-1
Tensile Strength at Break 4.50 MPa653 psiISO 527-1
Tensile Strength, Yield 0.700 MPa
@Strain 10.0 %
102 psi
@Strain 10.0 %
DIN EN ISO 527-1
Elongation at Break 500 %500 %ISO 527-1
50% Modulus 1.65 MPa
@Strain 50.0 %
1.65 MPa
@Strain 50.0 %
DIN EN ISO 527-1
100% Modulus 2.20 MPa
@Strain 100 %
319 psi
@Strain 100 %
DIN EN ISO 527-1
300% Modulus 3.60 MPa
@Strain 300 %
522 psi
@Strain 300 %
DIN EN ISO 527-1
Tear Strength 7.00 kN/m39.9 pliDIN ISO 34-1
Compression Set  27.0 %
@Treatment Temp. 23.0 °C
27.0 %
@Treatment Temp. 73.4 °F
ISO 815-1
 55.0 %
@Treatment Temp. 70.0 °C
55.0 %
@Treatment Temp. 158 °F
ISO 815-1
 73.0 %
@Treatment Temp. 100 °C
73.0 %
@Treatment Temp. 212 °F
ISO 815-1
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  HB
@Thickness 0.400 mm
HB
@Thickness 0.0157 in
IEC 60695-11-10
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 250 °C428 - 482 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.0200 %<= 0.0200 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO624 / 326698

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.