MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow Tyrin® CM2136P Chlorinated Polyethylene Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: 36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible PVC in many uses. Can be calendered, injection molded, or extruded into tough, chemical and weather resistant products that can also provide built-in ignition resistance.

Performance highlights include: inherent flexibility with plasticization; inherent chemical and ignition resistance; compatibility with PVC, PE, SAN, ABS, and other polymers, excellent low temperature properties, resistance to weathering, acceptance of fillers and heat/light stabilizers.

Key Words: Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Vapor Transmission 1.80 cc-mm/m²-24hr-atm36% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Oxygen Transmission 32.0 cc-mm/m²-24hr-atm36% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Viscosity 20000 cPNominal melt viscosity. DuPont Dow test method CPE-D3
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 23.0 MPatypical Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Elongation at Break 425 %typical Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
100% Modulus 0.00140 GPa
@Strain 100 %
Unfilled Tyrin compound; ASTM D412
Tear Strength Test 180Unfilled Tyrin compound; ASTM D1004
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+13 ohm-cm
Dielectric Constant 5.1
@Frequency 10000 Hz
 6.1
@Frequency 100 Hz
Dissipation Factor 0.010
@Frequency 100 Hz
 0.10
@Frequency 10000 Hz
36% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 93.0 - 106 °Cfor extrusion
Middle Barrel Temperature 106 - 149 °Cfor extrusion
Front Barrel Temperature 149 - 162 °Cfor extrusion
Nozzle Temperature 162 °CExtrusion die
Melt Temperature 177 °CExtrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Tyrin® 3623A Chlorinated Polyethylene Elastomer
Dow Tyrin® 3611P Chlorinated Polyethylene Elastomer
Dow Tyrin® CM0836 Chlorinated Polyethylene Elastomer
Dow Tyrin® 4211P Chlorinated Polyethylene Elastomer
Dow Tyrin® CM0136 Chlorinated Polyethylene Elastomer

PDVI04 / 34178

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.