System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Durethan® BM 230 H2.0 901510 Nylon 6 (PA6), 30% Mineral Filled, Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 30% Mineral Filled
Material Notes:
PA 6, injection molding, 30% mineral, isotropic properties, heat-aging stabilized
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Bulk Density
0.800
g/cc
ISO 60
Density
1.36
g/cc
ISO 1183
Moisture Absorption at Equilibrium
2.2 %
50% RH; ISO 62
Water Absorption at Saturation
7.0 %
IOS 62
Linear Mold Shrinkage, Flow
0.0108
cm/cm
150x105x3; 280 °C / MT 80 °C; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0112
cm/cm
150x105x3; 280 °C / MT 80 °C; 500 bar; ISO 294-4
Mechanical Properties
Original Value
Comments
Puncture Resistance
1132
N
@Temperature -30.0 °C
ISO 6603-2
4694
N
@Temperature 23.0 °C
ISO 6603-2
Ball Indentation Hardness
180
MPa
ISO 2093-1
Tensile Strength at Break
80.0
MPa
5 mm/min; ISO 527-1,-2
Elongation at Break
10 %
5 mm/min; ISO 527-1,-2
Tensile Modulus
5000
MPa
1 mm/min; ISO 527-1,-2
Flexural Strength
140
MPa
2 mm/min; ISO 178-A
Flexural Yield Strength
130
MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus
4700
MPa
2 mm/min; ISO 178-A
Flexural Strain at Break
5.5 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO)
80.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1U
122
kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched
80.0
kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
120
kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
<=
10.0
kJ/m²
@Temperature -40.0 °C
ISO 179 1eA
Puncture Energy
4.20
J
@Temperature -30.0 °C
ISO 6603-2
19.1
J
@Temperature 23.0 °C
ISO 6603-2
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+12
ohm-cm
IEC 60093
Surface Resistance
1.00e+16
ohm
IEC 60093
Dielectric Constant
3.9
@Frequency 1e+6 Hz
IEC 60250
4.3
@Frequency 100 Hz
IEC 60250
Dielectric Strength
29.0
kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor
0.0080
@Frequency 100 Hz
IEC 60250
0.018
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
200
V
Solution B; IEC 60112
525
V
Solution A; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
70.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow
90.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point
222
°C
10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi)
185
°C
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
70.0
°C
ISO 75-1,-2
Deflection Temperature at 8.0 MPa
50.0
°C
ISO 75-1,-2
Vicat Softening Point
>=
200
°C
@Load 5.10 kg
120°C/h; ISO 306
200
°C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 3.20 mm
Oxygen Index
25 %
Method A; ISO 4589-2
Glow Wire Flammability Index
650
°C
@Thickness 2.00 mm
IEC 60695-2-12
Shrinkage, MD
0.32 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction 150x105x3; ISO 294-4
Shrinkage, TD
0.30 %
@Treatment Temp. 120 °C,
Time 14400 sec
150x105x3; ISO 294-4
Processing Properties
Original Value
Comments
Melt Temperature
280
°C
injection molding
270
-
290
°C
Mold Temperature
80.0
°C
injection molding
80.0
-
120
°C
Drying Temperature
80.0
°C
Dry Time
2.00
-
6.00
hour
Moisture Content
0.030 - 0.12 %
Karl Fischer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Celanese Minlon® 73M40 NC010 PA6-MD40
EMS-Grivory Grilon® BM-30 PA6-MD30
Envalior Durethan® BM 230 H2.0 901510 Nylon 6 (PA6), 30% Mineral Filled, Conditioned
Celanese Zytel® 73G45L NC010 PA6-GF45
EMS-Grivory Grilon® BG-50 S PA6-GF50
PLANW9440 / 208273
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.