MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman Araldite GY 281 Bisphenol F Epoxy Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Weight per Epoxide (EEW, g/eq) 159 to 172. Max color is 4.

Comments/Applications: Unmodified, low viscosity bis F epoxy, good flexibility. FDA listed. Used in coatings, adhesives, tank linings, flooring, filament winding, casting, pultrusion and RTM. Better chemical resistance than GY 6010 especially to organic solvents.

Data provided by Ciba Specialty Chemicals.

Ciba Specialty Chemicals has been acquired by Huntsman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 5000 - 7000 cP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman Araldite GY 282 Bisphenol F Epoxy Resin
Bakelite® EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Solvay CYCOM® 5276-1 Epoxy with G40-800 Tape Composite
DSM Somos® ProtoGen™ 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
Solvay CYCOM® 970 Epoxy - Carbon Fiber Reinforced Unidirectional Tape

PCIB52 / 28451

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.