SMC LPA 6703 LW NEUTRO is a sheet molding compound based on an unsaturated polyester resin class “A” grade reinforced with glass fibers. This SMC has been developed for body panel application, with low density, good mechanical properties and excellent surface. Good varnish adhesion and excellent gluing are other peculiarities of SMC LPA 6703 LW NEUTRO. SMC LPA 6703 LW NEUTRO is formulated according to RoHS, REAC regulation (SVHC) and WEEE European legislation.Information provided by Polynt Composites. |