MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Hostalen ACP 7740 F2 High Density Polyethylene (HDPE), Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Hostalen ACP 7740 F2 is a high density polyethylene having medium molar mass and a narrow molar mass distribution for production of tapes. Hostalen ACP 7740 F2 is appreciated by customers for converting on all tape stretching and film stretching lines to produce products with high tensile strength, high elongation at break and low tendency to fibrillation. Typical customer applications: protective netting in agriculture and building industry, slit film & tapes, round bale nets. This product is not intended for use in medical and pharmaceutical applications. Applications: Geotextile & Agriculture, Nets, Raffia/Tapes/Strapping

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³ISO 1183-1
Melt Flow  1.8 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.8 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 23 g/10 min
@Load 21.6 kg,
Temperature 190 °C
23 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.0 MPa3480 psiISO 527-1,-2
Tensile Modulus 1.00 GPa145 ksiISO 527-1,-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FISO 3146
Vicat Softening Point 75.0 °C167 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 230 °C356 - 446 °FInjection Molding Temperature
 
Descriptive Properties
Processing MethodBlown Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQT8455 / 220090

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.