MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Key Features:
  • For potting and encapsulation
  • Serviceable up to 400°F
  • Superior chemical resistance
  • Excellent electrical insulation properties
  • Minimal shrinkage and stress development
  • Resists thermal cycling and mechanical shocks
Product Description: Master Bond EP39MHT is a low viscosity, two component, epoxy system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to an exceptionally tough and thermally stable thermosetting polymer featuring outstanding electrical insulation properties and remarkably high resistance to thermal shocks and mechanical vibration. EP39MHT also features inertness upon exposure to water and a wide range of chemicals plus capability for sustained service at temperatures up to as high as 400°F. As it develops very little heat during curing, it is particularly desirable for casting thick sections with complicated geometrical configurations up to several inches as well as thin sections with minimal shrinkage and stress development. EP39MHT is especially recommended for use in applications where cured assemblies must retain excellent electrical insulation and mechanical strength properties. This is true even upon exposure to adverse environmental conditions at both ambient and elevated temperatures in the presence of water, many organic solvents and other chemicals. The cured epoxy exhibits high resistance to thermal cycling and many chemicals including water, acids, bases and solvents such as ethyl alcohol, toluene, etc. Adhesion to both similar and dissimilar substrates such as metals, glass, ceramics, vulcanized rubbers and many plastics is excellent. The color for Part “A” is clear and Part “B” is amber. EP39MHT is widely used in the electronics, electrical, computer, construction, metalworking, appliance, automotive and chemical industries. It has proven particularly successful for potting and encapsulation electronic assemblies with complicated geometrical configuration which are subject to thermal cycling and/or mechanical vibrations in adverse environments.

Product Advantages:

  • Convenient, non critical, easy to use, one to one mix ratio, by weight or volume
  • Low viscosity material flows evenly and spreads; ideal for potting and encapsulating
  • Versatile cure schedules; ambient temperature or fast elevated temperature cure
  • Excellent adhesion to a variety substrates

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 200 - 300 cPmixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70 - 80
Tensile Strength >= 7500 psi
Flexural Strength >= 9000 psi
Compressive Strength >= 10000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.2
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 93.3 °C
 48.0 - 72.0 hour
@Temperature 23.9 °C
Working Life 45.0 - 75.0 minAfter mixing, 100 g batch
Shelf Life 12.0 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Chemical Resistance0.0145Water resistance, 120 days immersion at 75°F, weight change
 0.017930% sulfuric acid, 120 days immersion at 75°F, weight change
 0.51Ethanol, 120 days immersion at 75°F, weight change
 0.64Toluene, 120 days immersion at 75°F, weight change
 1.4810% sodium hydroxide, 120 days immersion at 75°F, weight change
 3.42510% nitric acid, 120 days immersion at 75°F, weight change
Mixing Ratio1:1 by weight or volumeParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP19HT One Component, Storage Stable Epoxy
Kaneka Kane Ace MX-418 Multifunctional Epoxy Resin
Kaneka Kane Ace MX-395M75 Epoxy Resin
Kaneka Kane Ace MX-236 Multifunctional Epoxy Resin
Kaneka Kane Ace MX-227M75 Epoxy Resin

PMASTM875 / 185468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.