MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Westlake HIFOR® LF2041AA Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: HIFOR® LF2041 is a hexene LLDPE designed for cast film extrusion. HIFOR® LF2041 contains stabilization ideal for the cast extrusion process.

Test specimens for blown film: nominal thickness 1.0 mils; blow up ratio 2.5:1, die gap 100 mils at 50% relative humidity and 23°C.

Information provided by Westlake Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Melt Index of Compound 2.0 g/10 min2.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 450 %450 %ASTM D882
Film Elongation at Break, TD 800 %800 %ASTM D882
Elmendorf Tear Strength, MD 7.87 g/micron200 g/milASTM D1922
Elmendorf Tear Strength, TD 25.6 g/micron650 g/milASTM D1922
Dart Drop 3.54 g/micron90.0 g/milASTM D1709
Film Tensile Strength at Break, MD 35.9 MPa5200 psiASTM D882
Film Tensile Strength at Break, TD 20.7 MPa3000 psiASTM D882
1% Secant Modulus, MD 152 MPa22000 psiASTM D882
1% Secant Modulus, TD 172 MPa25000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 2.5 %2.5 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 282 °C500 - 540 °FCast extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF8744 / 287854

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.