MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Polymist® XPP 511 R PTFE, Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: Polymist® XPP 511 R is a medium MW grade of micronized PTFE with coarse particle size and excellent thermal stability.

It is designed for use in critical, high temperature engineering and high performance polymers to provide improved wear resistance and low coefficient of friction.

Main features of Polymist® XPP 511 R are:
- Better wear resistance
- Increased pressure x velocity (PV) limits
- Reduced friction
- Improved stick-slip response
- Improved mold release

Applications: Additive

Processing
Polymist® XPP 511 R can be used in a wide variety of different thermoplastics. Typical loadings are 5 - 20% by weight of the compound and the optimum loading is dependent by the resin type and the desired final properties of the part.

Besides its main function as a friction and wear additive, Polymist® XPP 511 R micronized powders can be also used at lower concentration to provide the following properties:
- Processing aid to improve compounding and molding conditions
- Mold release agent due to non-stick properties

Polymist® XPP 511 R micronized PTFE can be incorporated into thermoplastics by pre-mixing or co-feeding with the base polymer using standard industrial equipment and technology. The compound can also be prepared by first using a masterbatch.

Storage and Handling
- The usual precautions for safe storage and handling of Polymist® XPP 511 R should be taken according to material safety documentation and experience. There will be no chemical deterioration of the Polymist® XPP 511 R during proper storage.

- Shelf life of Polymist® XPP 511 R micronized powders will vary depending upon whether the recommended storage conditions are maintained and whether the material remains free from foreign contamination during storage time (not exposed to dirt, dust, water or other chemicals). The material should remain sealed in the original containers and storage conditions should provide for protection from temperature extremes as well as rain, snow or other wet environments (or such conditions which may damage the storage containers in which the product is stored).

Safety and Toxicology
- Before using PTFE Polymist® XPP 511 R micronized powders consult the product Material Safety Data Sheet and follow all label directions and handling precautions.

- As with all PTFE materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapor or fumes.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³ASTM D4894
Particle Size 20 µm20 µm
Specific Surface Area 3.0 m²/g3.0 m²/g
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
ColorWhite
FormsPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4378 / 280178

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.