MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics Tecknit Teckfip™ FIP-X Formed in Place Conductive Elastomer
Categories: Polymer

Material Notes: FIP-X features a conductive powder that is a unique particle combining tungsten carbide and aluminum. The premium advantage of this compound is its ability to be non-corrosive even in the most hostile of external environments. The compound has been exhaustively tested for hostile environments and easily exceeds the requirements of the ASTM B117 test specification. Tecknit also offers a flame-retardant version of this compound which has achieved the UL94-V0 rating.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.479 - 2.001 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 57 - 73
Tensile Strength 215 psi
Elongation at Break >= 90 %
Peel Strength >= 9.00 kN/m
Compression Set 25 %Recommended
 10 - 50 %
 31 %
@Temperature 70.0 °C,
Time 79200 sec
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.031 ohm-cm
Surface Resistance 1.5 ohm[ohm-cm]
 0.046 ohm
@Temperature 85.0 °C,
Time 605000 sec
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -55.0 °C
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Cure Time <= 24.0 hour
Tack-Free Time >= 0.200 hour
Shelf Life 1.00 MonthSyringe
 6.00 MonthCartridge
 
Descriptive Properties
ColorDark Gray
FillerTungsten Carbide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A131 Steel, Grade AH36
ASTM A572 Steel, grade 50
Latrobe LSS™ A6 Tool Steel (ASTM A6)
ASTM A529 Steel
AISI Type A6 Tool Steel

PCHOME355 / 131065

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.