MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Parson Adhesives PARFIX® 3499 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PARFIX 3499 is high viscosity combined with fast cure speed, and excellent thermal resistant cyanoacrylate adhesive. It is specifically formulated to bond various Rubbers, Metals and Plastics for use in challenging environments.

Applications:

  • Ideal for bonding Rubbers, Metals and Plastics.
  • Excellent hot strength and heat aging capabilities at temperatures up to 120°C for periods in excess of 3000 hours.
  • Ideal for Speaker Assemblies, Automotive Components, Electrical Equipment, Oil Filters and Disk Drives.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 7.03 MPa>= 1020 psiPolycarbonate; ASTM D1002
 >= 10.0 MPa>= 1450 psiSBR Rubber; ASTM D1002
 >= 10.0 MPa>= 1450 psiPVC; ASTM D1002
 >= 12.0 MPa>= 1740 psiNeoprene Rubber; ASTM D1002
 >= 12.0 MPa>= 1740 psiNitrile Rubber; ASTM D1002
 >= 16.0 MPa>= 2320 psiAluminum; ASTM D1002
 13.0 - 25.0 MPa1890 - 3630 psi
 >= 20.0 MPa>= 2900 psiSteel; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.32.3ASTM D150
Dielectric Strength 32.5 kV/mm825 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 310 µm/m-°C172 µin/in-°FASTM D696
Melting Point 160 - 170 °C320 - 338 °F
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 165 °C329 °FASTM E228
Flash Point >= 80.0 °C>= 176 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.167 - 0.330 min0.00278 - 0.00550 hourSBR Rubber
 0.250 - 0.330 min0.00417 - 0.00550 hourAluminum
 0.250 - 0.330 min0.00417 - 0.00550 hourNeoprene Rubber
 0.250 - 0.330 min0.00417 - 0.00550 hourNitrile Rubber
 0.330 - 0.4167 min0.00550 - 0.006945 hourPolyurethane Rubber
 0.417 - 0.583 min0.00695 - 0.00972 hourPhenolic Materials
 0.500 - 1.33 min0.00833 - 0.0222 hourEPDM
 1.00 - 1.167 min0.0167 - 0.01945 hourSteel
 1440 min24.0 hourFull
 
Descriptive Properties
AppearanceClear liquid
CompositionRubber Toughened Ethyl Cyanoacrylate
Gap Filling0.7 mm
Initial Strength Retained (%)75Gasoline for 1000 hrs at 22°C
 80Gasoline for 500 hrs at 22°C
 85Isopropanol for 500 hrs at 22°C
 85Isopropanol for 1000 hrs at 22°C
 90Motor Oil for 500 hrs at 40°C
 90Motor Oil for 1000 hrs at 40°C
 90Mineral Spirit for 500 hrs at 22°C
 90Mineral Spirit for 1000 hrs at 22°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPARSN140 / 186583

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.