MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos H12Z-00 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: This is a nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

    Applications
  • Closures, lids, and overcaps
  • Consumer products
  • Furniture
  • Housewares
  • Rigid packaging

    Benefits
  • Fast cycle times
  • Improved stiffness
  • Low static charge

Information provided by Ineos Olefins & Polymers USA

Key Words: Nucleated and antistatic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.914 g/cc0.0330 lb/in³ASTM D792
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103ASTM D785
Tensile Strength at Break 18.0 MPa2610 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 37.4 MPa5430 psi2.0 in/min; ASTM D638
Elongation at Break 78 %78 %2.0 in/min; ASTM D638
Elongation at Yield 8.6 %8.6 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1830 MPa266000 psiASTM D790A
Izod Impact, Notched 0.374 J/cm0.700 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 3.80 kJ/m²1.81 ft-lb/in²Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 3.05 mm
HB
@Thickness 0.120 in
 
Optical PropertiesMetricEnglishComments
Haze 55 %
@Thickness 1.27 mm
55 %
@Thickness 0.0500 in
ASTM D1003
Gloss 92 %92 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ProcessInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPH 3620WZ Polypropylene, Injection Molding Grade
Flint Hills P4C6B-134A Polypropylene Homopolymer
Ineos H02C-00 Polypropylene Homopolymer
LyondellBasell Pro-fax 6523 Polypropylene Homopolymer, General Purpose
Braskem D115A Homopolymer Polypropylene

PINEOS036 / 99357

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.