MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Dover Chemical DOVERPHOS S9228PC Solid Phosphite Antioxidant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Doverphos S-9228PC is a free flowing solid phosphite antioxidant developed by 1057. Doverphos S-9228PC has excellent hydrolytic stability without the addition of inert products or triisopropanol amine. Doverphos S-9228PC exhibits excellent color performance. Because of its high melting point, Doverphos S-9228PC can be utilized in applications that require processing at elevated temperatures.

Information provided by DoverChem

Key Words: CAS# 154862-43-9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 852 g/mol852 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 225 °C>= 437 °F
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 7.3 %7.3 %
Sodium, Na <= 0.0050 %<= 0.0050 %
 
Descriptive Properties
AppearanceOff White
Physical FormFree Flowing Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDOVER047 / 217666

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.