Adflex Z 101 H is a reactor TPO (thermoplastic polyolefin) manufactured using the LyondellBasell’s proprietary Catalloy process technology. It exhibits high softness and low modulus, with high melt flow index. Adflex Z 101 H is tailored to replace atactic polypropylene copolymers (APP) used for the modification of bitumen in roofing membranes. The percentage to be added can vary according to the quantity of the atactic polypropylene used in combination with Adflex Z 101 H and the requested cold bending temperature of the end product. Its structure is tailored to obtain easy dispersion and phase inversion in the bitumen blend. The grade is available in natural pellet form. Applications: Bitumen Modification, Carpet Backing, Impact Modification, Nonwovens, Soft Touch Applications.Information provided by LyondellBasell. |