MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics PPS Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: The linear polyphenylene sulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional stability, and creep strength. The LOI belongs to the highest of polymers. By the reinforcement with glass polymers strength is achieved, which is comparable with light metal. PPS closes the gap between the technical synthetics and PEEK with its strength and economy.

Properties

  • very high strength and rigidity
  • high hardness
  • high thermostability
  • high dimensional stability
  • very high chemical resistance
  • very good insulating properties
  • high weather resistance
  • high resistance to hydrolysis
Applications include components in machine-making, pump parts, fan parts, impellers, parts in the fuel and automotive sector.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccISO 1183
Moisture Absorption at Equilibrium 0.010 %ISO 62
Water Absorption at Saturation 0.020 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ISO 2039
Hardness, Shore D 88ISO 868
Ball Indentation Hardness 246 MPaISO 2039
Tensile Strength at Break 88.0 MPaISO 527
Tensile Strength, Yield 94.0 MPaISO 527
Elongation at Break 8.0 %ISO 527
Modulus of Elasticity 3.70 GPaISO 527
Flexural Strength 143 MPaISO 178
Charpy Impact Unnotched 28.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+11 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 30.0 kV/mmIEC 60243-1
Comparative Tracking Index 125 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 58.0 µm/m-°CISO 11359
Thermal Conductivity 0.250 W/m-K
@Temperature 20.0 °C
ISO 22007-4
Melting Point 280 °CDIN EN ISO 3146
Maximum Service Temperature, Air 230 °CUL 746B
Deflection Temperature at 1.8 MPa (264 psi) 115 °CISO 75
Glass Transition Temp, Tg 97.0 °CDIN EN ISO 3146
Flammability, UL94 V-0UL 94
Oxygen Index 47 %ASTM D2863
 
Compliance PropertiesOriginal ValueComments
FDA YesPhysiological indifference
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistancelimited
Bondabilityyes
CKW Resistanceyes
Colornatural
Hydrocarbonate Resistanceyes
Hydroxide Resistancelimited
Ketone Resistanceyes
Physiological indifferenceyes, EEC
Resistance Against Hot Wateryes
UV Stabilizationlimited

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CENTROPLAST CENTROTRON Polyphenylene sulfide
Ensinger TECATRON™ PPS Polyphenylene sulfide (PPS)
Evonik Vestamid® L-GB30 15% Carbon Fiber Filled Nylon 12
GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber
CENTROPLAST CENTROFLON Polyvinylidene fluoride

PGEHR035 / 79872

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.