MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Aluminum Bronze, UNS C95200, Copper Casting Alloy, M05 Temper, As Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Permanent Mold Cast

Casting Characteristics: High – Drossing, Shrinkage in Solidification, Shrinkage During Freezing; Medium – Fluidity, Gassing; Low - Casting Yield, Effect of Section Size

Fabrication Properties: Excellent Suitability – Gas Shielded Arc Welding; Good Suitability – Soldering, Brazing, Coated Metal Arc Welding

Typical uses: Electrical Hardware; Nuts; Acid Resistant Pumps; Bearing Liners; Bearings; Gears; High Strength Clamps; Hot Mill Guides; Hydrant Parts; Large Gear Parts; Mild Alkali Applications; Pickling Equipment; Pickling Tanks; Plungers; Pump Parts; Thrust Pads; Valve Bodies; Valve Seats; Valves; Wear Plates; Welding Jaws; Worm Wheels; Worms; Covers for Marine Hardware; Marine Engines; Marine Hardware; Propellers; Gun Mountings; Gun Slides

Applicable Specifications: As Centrifugal Cast – Castings SAE J461, Castings ASME SB271, Castings SAE J462, Castings ASTM B271/B271M; As Continuous Cast – Castings SAE J461, Castings ASME SB505, Castings SAE B505/B505M Castings ASTM B505/B505M; As Sand Cast – Castings ASME SB148; Castings ASTM B763/B763M, Castings SAE J462, Castings SAE J461, Castings ASTM B148; Flanges – ASME B16.24, ASME SB148, ASTM B148; Ingot - ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.64 g/cc0.276 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7878
Tensile Strength 641 MPa93000 psi
Tensile Strength, Yield 241 MPa35000 psi
Elongation at Break 38 %38 %
Tensile Modulus 103 GPa15000 ksi
Modulus of Rigidity 39.47 GPa5725 ksiCalculated
Poissons Ratio 0.310.31
Machinability 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000156 ohm-cm0.0000156 ohm-cm11% IACS
Magnetic Permeability 1.11.1Field Strength 16000 A/m(200 Oersteds)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 4.19 W/m-K29.1 BTU-in/hr-ft²-°F
Melting Point 1042 - 1045 °C1907 - 1913 °F
Solidus 1042 °C1907 °F
Liquidus 1045 °C1913 °F
Shrinkage 2.08 %2.08 %Patternmaker's Shrinkage (4/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 316 °C600 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.5 - 9.5 %8.5 - 9.5 %
Copper, Cu >= 86 %>= 86 %
Iron, Fe 2.5 - 4.0 %2.5 - 4.0 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC95200x3 / 293244

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.