MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SLArmor Protoyping Composite System, 10% Nickel
Categories: Metal

Material Notes: SLArmor is a process/material combination used to produce SLA parts consisting of a plated nickel over DSM Somos NanoTool. The parts are similar to die cast aluminum with excellent stiffness and high strength, and can be used for protoyping of cast metals parts such as Al, Mg, or Zn.

The core material is a ceramic filled composite; parts are subsequently electroform-plated with a structural layer of nickel.

Property data below is a for a system of 10% metal by volume, although geometry plays a significant role in the final properties of a real world component.

Information provided by FineLine, a Proto Labs Service.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.33 g/cc0.0842 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psiASTM D638M
Elongation at Break 0.9 %0.9 %ASTM D638M
Tensile Modulus 21.0 GPa3050 ksiASTM D638M
Flexural Strength 300 MPa43500 psiASTM D790M
Flexural Modulus 28.0 GPa4060 ksiASTM D790M

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NiCoForm NiColoy® E Electroformed Nickel-Cobalt
Aluminum A360.0-F Die Casting Alloy
Aluminum A380.0-F Die Casting Alloy
Overview of materials for Cobalt Alloy
Special Metals Electroformed Nickel, 200 Micron (8 mil) Foil, Electroformed and Annealed

PPROTL991 / 191505

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.