MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SACO AEI EXTINITY® 0218-108 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: EXTINITY® 0218-108 is a highly loaded flame-retardant concentrate that can be used for a variety of polystyrene-based applications. This concentrate has been designed to be used in High Impact Polystyrene, but is also effective in the entire styrenic family including general purpose polystyrene grades. EXTINITY® 0218-108 provides excellent flame-retardant performance while having minimal impact on mechanical properties and processibility. Varying the use rate of 0218-108 will permit the final compound to meet UL-94 V-0, V-1 or V-2 requirements.

Recommended Applications:
Extrusion: Profile, Sheet
Molding: Injection

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D792
Storage Temperature -12.2 - -3.89 °C10.0 - 25.0 °F
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  V-2
@Thickness 1.59 mm
V-2
@Thickness 0.0625 in
 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 380 - 450 °C716 - 842 °F
 
Descriptive Properties
FormNatural Pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSACO035 / 249402

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.