System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Lubrizol Estane® S364D Thermoplastic Polyurethane
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
;
Thermoplastic Polyurethane (TPUR), Polyester Grade
Material Notes:
Type:
Estane® S364D is a Shore 65D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).
Uses:
Injection Molding.
Availability: Asia
Information Provided by The Lubrizol Corporation
Key Words:
TPU
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.25
g/cc
ASTM D792
Linear Mold Shrinkage
0.0040
cm/cm
ASTM D955
Mechanical Properties
Original Value
Comments
Hardness, Shore D
65
ASTM D2240
Tensile Strength, Ultimate
440
kg(f)/cm²
ASTM D412
Tensile Strength, Yield
240
kg(f)/cm²
at 100% elongation; ASTM D412
390
kg(f)/cm²
at 300% elongation; ASTM D412
Elongation at Break
390 %
ASTM D412
Tear Strength
220
kg(f)/cm
Die C; ASTM D624
Abrasion
30
mm
3
loss; ISO 4649
Compression Set
20 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395
40 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
Thermal Properties
Original Value
Comments
Vicat Softening Point
123
°C
ASTM D1525
Processing Properties
Original Value
Comments
Feed Temperature
200
-
215
°C
Nozzle Temperature
215
-
230
°C
Mold Temperature
10.0
-
40.0
°C
Drying Temperature
70.0
-
80.0
°C
Dry Time
4.00
-
5.00
hour
Injection Pressure
1800
-
2400
psi
Hold Pressure
1300
-
1900
psi
Back Pressure
30.0
-
80.0
psi
Cycle Time - Injection
25
-
30
sec
Screw Speed
160
-
200
rpm
Compliance Properties
Original Value
Comments
FDA
Yes
Descriptive Properties
Injection Time (s)
12-18
Metering Zone
210-225°C
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Lubrizol Estane® S375D Thermoplastic Polyurethane
Lubrizol Estane® S368D Thermoplastic Polyurethane
Wanhua Chemical Wanthane® WHT-8290 Polyether-Based TPU
Wanhua Chemical Wanthane® WHT-7195 Polycaprolactone Based TPU
Wanhua Chemical Wanthane® WHT-1180H Super Hard Polyester Based TPU
PNOVEON524 / 121415
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.