MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.

Benefits: The product is particularly recommended for the molding of parts where some translucency is required, as well as surface aesthetics is important.

Available in: North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: This grade is particularly recommended for the injection molding of parts in permanent contact with cooling liquids in cars, such as reservoir bottles.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 190 MPaISO 527 Type 1A
Tensile Stress at Strain 25.0 MPa
@Strain 1 %,
Temperature 150 °C
 35.0 MPa
@Strain 1 %,
Temperature 100 °C
 45.0 MPa
@Strain 2 %,
Temperature 150 °C
 55.0 MPa
@Strain 3 %,
Temperature 150 °C
 60.0 MPa
@Strain 2 %,
Temperature 100 °C
 60.0 MPa
@Strain 4 %,
Temperature 150 °C
 70.0 MPa
@Strain 6.0 %,
Temperature 150 °C
 75.0 MPa
@Strain 10 %,
Temperature 150 °C
 80.0 MPa
@Strain 3 %,
Temperature 100 °C
 85.0 MPa
@Strain 4 %,
Temperature 100 °C
 90.0 MPa
@Strain 1 %,
Temperature 23.0 °C
 95.0 MPa
@Strain 6.0 %,
Temperature 100 °C
 100 MPa
@Strain 10 %,
Temperature 100 °C
 105 MPa
@Strain 1 %,
Temperature -40.0 °C
 155 MPa
@Strain 2 %,
Temperature 23.0 °C
 180 MPa
@Strain 2 %,
Temperature -40.0 °C
 180 MPa
@Strain 3 %,
Temperature 23.0 °C
 220 MPa
@Strain 3 %,
Temperature -40.0 °C
Elongation at Break 3.8 %ISO 527 Type 1A
Tensile Modulus 10200 MPaISO 527 Type 1A
Flexural Strength 294 MPaISO 178
Flexural Modulus 8950 MPaISO 178
Izod Impact, Notched (ISO) 11.3 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 90.7 kJ/m²ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 263 °CISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 247 °CISO 75/Af
 
Processing PropertiesOriginal ValueComments
Feed Temperature 255 - 265 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone265-275°C
Mixing Zone275-280°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium, Mg; Hard-Rolled Sheet
Domo Technyl® A218GV33-BK 33% Glass Filled, Heat Stabilized, Hydrolysis Resistant, Black Nylon 66
Domo TECHNYL® A 218G V33 Black 41N PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY
Domo TECHNYL® A 218 PA66, 33% glass fiber, DRY

PRHOD682 / 137913

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.