Description: Metlbond 1515-4 is a 350°F (177°C) curing modified epoxy supported film adhesives. Metlbond 1515-4 can also be cured at 250°F (121°C). Its maximum continuous service temperature range is 275°F to 320°F (135°C to 160°C). Metlbond 1515-4 is commonly used for Boeing BMS 5-154 metal-to-metal and composite bonding and BMS 8-341 cosmetic surfacing. Features & Benefits: - Extended shop life of 30 days at up to 90°F (32°C) allows lay up of large components
- Designed for co-curing, secondary bonding, and co-bonding of composite materials
- Provides excellent surfacing characteristics
- Good resistance to pre-cure humidity
- Available in a variety of weights and carriers
- Bonds metal-to-metal, metal-to-core and composites
- Co-Note 1: Metlbond 1515-4, BMS 5-154, Pre-exposed Film 30 days at 90°F (32°C) and 50% R.H.cures with most 350°F (177°C) curing prepregs
- Storage life of 12 months at 0°F (-18°C)
Applications: - Metal-to-metal bonding
- Composite bonding
- Cosmetic surfacing
Note 1: Metlbond 1515-4, BMS 5-154, Pre-exposed Film 30 days at 90°F (32°C) and 50% R.H.Note 2: Metlbond 1515-4, BMS 5-154, Non Pre-exposed Film Information provided by Cytec, subsequently acquired by Solvay. |