MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Akulon® F127 PA6
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Low/Medium Viscosity, Film Extrusion

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Water Vapor Transmission 35.0 g/m²/day
@Temperature 23.0 °C
at 85% r.h., film; DIS 15106-1/-3
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm
@Temperature 23.0 °C
at 0% r.h., film; DIS 15105-1/-2
 1.90 cc-mm/m²-24hr-atm
@Temperature 23.0 °C
at 85% r.h., film; DIS 15105-1/-2
Viscosity 410000 cP
@Temperature 260 °C
Melt Viscosity; DSM method
 200000 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
 250000 cP
@Shear Rate 1000 1/s,
Temperature 260 °C
 300000 cP
@Shear Rate 1000 1/s,
Temperature 240 °C
 350000 cP
@Shear Rate 0.1 1/s,
Temperature 280 °C
 475000 cP
@Shear Rate 0.1 1/s,
Temperature 260 °C
 650000 cP
@Shear Rate 0.1 1/s,
Temperature 240 °C
Viscosity Measurement 2.7RSV formic acid, 1g/100ml; DSM method
Viscosity Number 168 cm³/gISO 307, 1157, 1628
Thickness 1.97 milfilm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 32.0 MPaparallel; ISO 527-3
Film Elongation at Break, MD 350 %parallel; ISO 527-3
Modulus of Elasticity 0.460 GPafilm; DSM-Method, 50 mm/min
Coefficient of Friction, Dynamic 1.2film; ISO 8295
Coefficient of Friction, Static 1.5film; ISO 8295
Tear Strength Test 32Trouser tear resistance, parallel, film; ISO 6383-1
Film Tensile Strength at Break, MD 80.0 MPaparallel; ISO 527-3
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°CISO 11359-1/-2
Specific Heat Capacity 1.55 J/g-°C
@Temperature 23.0 °C
 2.25 J/g-°C
@Temperature 20.0 - 150 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 83 %film; DSM method
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 °CExtruder Temperature
Die Temperature 270 °C
Roll Temperature 110 °C
 
Descriptive Properties
Extrusion TypeCast Film
Puncture Resistance1150 J/mFilm (DSM Method)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® F136 PA6
Envalior Akulon® F232 PA6
Envalior Akulon® F132 PA6
Envalior Akulon® F132-E1 PA6
Envalior Akulon® F136-E1 PA6

PDSM9751 / 161372

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.