MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese SO.F.TER Nylfor A® A2 FR1/2A Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Flame retardant polyamide 66, halogen and phosphorous free

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D1505
Water Absorption 7.5 %7.5 %ISO 62
Moisture Absorption at Equilibrium 2.2 %2.2 %ISO 62
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm0.0090 - 0.013 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 80.0 MPa11600 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Tensile Modulus 3.70 GPa537 ksiASTM D638
Flexural Modulus 3.30 GPa479 ksiASTM D790
Izod Impact, Notched 0.400 J/cm0.749 ft-lb/inASTM D256
Charpy Impact, Notched 0.450 J/cm²2.14 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FASTM D648
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 280 °C500 - 536 °FCylinder Temperature
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 90.0 °C
@Time 14400 sec
194 °F
@Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epsan Eplamid 66 GX0 25 RP Q1C5B601 Polyamide 66, Halogen Free
Ravago Manufacturing Americas Hylon® N1025HLFRA Nylon 66, 25% Glass Filled, Conditioned
Wellman Wellamid® FRGF25-66 NBK3 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant
RTP Company RTP 204 FR XB Nylon 6/6 (PA) Glass Fiber - Flame Retardant - Black Color Only
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant

PSOFS860 / 162324

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.