MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Pyrotek Pyrocast ZC Refractory Shapes
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Aggregate Base: Mullite

Applications

  • Door sill
  • Breech plug
  • Door jamb

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.74 g/cc0.0990 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 68.95 - 96.53 MPa10000 - 14000 psiafter 816°C
Abrasion 4.0 - 8.04.0 - 8.0Resistance (CC Loss) ASTM C704
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.12 µm/m-°C
@Temperature 20.0 °C
3.40 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 1.67 W/m-K
@Temperature 538 °C
11.6 BTU-in/hr-ft²-°F
@Temperature 1000 °F
Maximum Service Temperature, Air 1649 °C3000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Pyrocast ALF3 Low Cement Refractory Castable
Pyrotek Pyrocast HD Castable Refractory
Pyrotek Pyrocast PCR Abrasion-Resistant Refractory Castable
Pyrotek Pyrocast ZE Refractory Shapes
Pyrotek Pyrocast ZEAL Refractory Shapes

CPYRO188 / 1905

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.