  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Versalis Clearflex® FG 106 A Film Grade LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Clearflex® FG 106 A is a hexane copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion. Clearflex® FG 106 A properties include: superior film toughness and strength, potential down gauging, superior optical properties and outstanding sealing performance.

Application: Clearflex® FG 106 A is recommended for agricultural film, blown stretch film, barrier food packaging, form fill and seal packaging, lamination film. Improved toughness, excellent seal ability and high throughput are just some of the benefits which add value to our customers across the supply chain.

Property data reported for film extruded between 190°-230°C, with BUR 2.5, thickness 25 µm.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccISO 1183
Thickness 25.0 micronsAs tested
 10.0 - 50.0 micronsRecommended
Melt Flow 1.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 9.00 MPaISO 527-3
Film Tensile Strength at Yield, TD 10.0 MPaISO 527-3
Film Elongation at Break, MD 600 %ISO 527-3
Film Elongation at Break, TD 700 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50ISO 8295
Elmendorf Tear Strength, MD 13.3 g/micronISO 6383-2
Elmendorf Tear Strength, TD 23.5 g/micronISO 6383-2
Dart Drop Test 180 gF50; ISO 7765-1/A
Film Tensile Strength at Break, MD 50.0 MPaISO 527-3
Film Tensile Strength at Break, TD 45.0 MPaISO 527-3
1% Secant Modulus, MD 180 MPaISO 527-3
1% Secant Modulus, TD 210 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 125 °CManufacturer method
Vicat Softening Point 101 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -70.0 °CASTM D 746
 
Optical PropertiesOriginal ValueComments
Haze 8.0 %ISO 14782
Gloss 65 %45°; ASTM D 2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 230 °CAs Tested

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENF9827 / 265531

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.