MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sinpolene FRF2074 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Availability: Africa & Middle East; Latin America; Asia Pacific; South America

Features: Flame Retardant

Uses: Appliance Components; Housings

Forms: Pellets

Information Provided by Teknor Apex

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.938 g/cc0.938 g/ccASTM D792
Linear Mold Shrinkage 0.00013 cm/cm0.00013 in/inASTM D955
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8787ASTM D785
Tensile Strength, Yield 38.0 MPa5510 psiASTM D638
Flexural Strength 40.0 MPa5800 psiASTM D790
Flexural Modulus 1.30 GPa189 ksiASTM D790
Izod Impact, Notched 0.251 J/cm
@Temperature 22.8 °C
0.470 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FUnannealed; ASTM D648
Vicat Softening Point 154 °C309 °FLoading 1 (10N); ASTM D1525
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized, Copolymer Polypropylene
Tipco Tipcolene® PP FR V0 - UL94-V0 Flame Retardant Polypropylene Homopolymer
Techmer ES HiFill FR® PP FR-N X BKN001
SPS Guang Zhou SAMAT™ 5003 Flame-retarded Polypropylene
Overview of materials for Polypropylene, Flame Retardant

PTEKNP227 / 129308

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.