MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Copper Alloy, UNS C64752, H06 Temper, Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Extra Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding; Fair Suitability – Capacity for Being Hot Formed

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 265
@Load 3.00 kg
265
@Load 6.62 lb
Tensile Strength 827 - 931 MPa120000 - 135000 psi
 883 MPa128000 psiTypical
Tensile Strength, Yield 800 - 910 MPa116000 - 132000 psi0.2% Offset
 855 MPa124000 psi0.2% Offset, Typical
Elongation at Break >= 1.0 %>= 1.0 %
Tensile Modulus 130 GPa18900 ksi
Modulus of Rigidity 48.99 GPa7105 ksiCalculated
Poissons Ratio 0.330.33
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000540 ohm-cm0.00000540 ohm-cm32% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.3 µm/m-°C
@Temperature 20.0 - 300 °C
9.61 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 12.8 W/m-K89.0 BTU-in/hr-ft²-°F
Melting Point 1050 - 1078 °C1930 - 1972 °F
Solidus 1050 °C1930 °F
Liquidus 1078 °C1972 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 94 - 96.4 %94 - 96.4 %As Balance
Nickel, Ni 2.8 - 3.8 %2.8 - 3.8 %
Phosphorus, P 0.0050 - 0.050 %0.0050 - 0.050 %
Silicon, Si 0.60 - 1.2 %0.60 - 1.2 %
Tin, Sn 0.15 - 1.0 %0.15 - 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC64752x1 / 292236

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.