Main characteristics: • High toughness even at low temperatures • High dimensional accuracy and stability • Good paintability • Good flowabilityGrade characteristics: • Flame retardant As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |