MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Vacupor® PR-B2-S Porextherm
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Vacupor® RP-B2-S is a microporous insulation material which has an extremely low coefficient of thermal conductivity, i.e. with very good insulating properties. Vacupor® RP-B2-S consists of inorganic oxides. The main constituent is fumed silica, the other components are opacifiers for minimizing infrared radiation, and fiber filaments as reinforcing fillers. Vacupor® RP-B2-S is approved by DIBT under the certification number Z-23.11-1662.The approval is valid for construction applications DAD, DAA, DZ and DEO, according to standard DIN 4108-10 and prefabricated façade panels with insulated glass character. Vacupor® RP-B2-S conforms to building material class E (B2). The test of behaviour in case of fire according DIN 4102-1, May 1998, building material class B2; test certificate no. H.3-145/07 and H.3-146/07, was issued by the Forschungsinstitut für Wärmeschutz e.V. München. The core material of Vacupor® RP-B2-S is not flammable and is classified A1 according to DIN ISO EN 13501-1. Vacupor® RP-B2-S is heat sealed in a multilayer vacuum metalised film. The very low internal pressure and the microporous panel core enable it to reach extremely low thermal conductivity values.

Application: Vacupor® RP-B2-S was specially developed for applications in the building,and construction industry where an approval by the building authorities is required. The low density and IR opacifiers contained in these grades greatly reduce the thermal conductivity of Vacupor® RP-B2-S Systems. Due to the single- or double-sided coverage with a rubber protection layer, Vacupor® RP-B2-S is particularly suitable for all kinds of plane linings. The fixing of the insulation is much easier, and the VIPs can be installed without any damage being caused. The fixing of the insulation is ubstantially facilitated, through the possibility of bonding with commercial solvent free adhesives.

Typical applications: Vacupor® RP-B2-S is successfully used as insulation material in the following areas:

  • Terrace insulation
  • Cold storage floor insulation
  • Floor insulation
  • Flat roof insulation

Information provided by Morgan Advanced Materials

Key Words: Porextherm
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.170 - 0.210 g/cc0.00614 - 0.00759 lb/in³depending on thickness
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 1.00 MPa145 psiat 210 kg/m3
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.00700 W/m-K0.0486 BTU-in/hr-ft²-°Frated value. According to DIBt general approval no. Z-23.11-16.
 <= 0.0190 W/m-K<= 0.132 BTU-in/hr-ft²-°Fat ambient pressure.
 0.00363 W/m-K
@Pressure 1.00e-7 MPa
0.0252 BTU-in/hr-ft²-°F
@Pressure 0.0000145 psi
 0.00366 W/m-K
@Pressure 0.0000100 MPa
0.0254 BTU-in/hr-ft²-°F
@Pressure 0.00145 psi
 0.00375 W/m-K
@Pressure 0.000100 MPa
0.0260 BTU-in/hr-ft²-°F
@Pressure 0.0145 psi
 0.00425 W/m-K
@Pressure 0.00100 MPa
0.0295 BTU-in/hr-ft²-°F
@Pressure 0.145 psi
 0.00870 W/m-K
@Pressure 0.0150 MPa
0.0604 BTU-in/hr-ft²-°F
@Pressure 2.18 psi
 0.0183 W/m-K
@Pressure 0.100 MPa
0.127 BTU-in/hr-ft²-°F
@Pressure 14.5 psi
 <= 0.00500 W/m-K
@Pressure 0.100 MPa,
Temperature 22.5 °C
<= 0.0347 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 72.5 °F
Maximum Service Temperature, Air <= 120 °C<= 248 °FThe limits are fixed by the barrier film; durable maximum temperature is at 80°C; short time maximum at 120°C for approximately 30 minutes.
Minimum Service Temperature, Air >= -50.0 °C>= -58.0 °F
 
Descriptive Properties
Colorsilver/black
Compression Behavior (%)10at 1 bar, 160kg/m3
 10at 3 bar, 230 kg/m3
 15at 2 bar, 160 kg/m3
 20at 3 bar, 160 kg/m3
 5at 1 bar, 230kg/m3
 8at 2 bar, 230 kg/m3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool® Rigidizer Coating
3D Systems DuraForm® AF Nylon for SLS® Systems

CMORF6122 / 202906

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.