MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kazanorgsintez P2ES-12 Electrically Conductive Polyethylene Composite
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Production Method: P2ES-12 is produced from low density polyethylene, modified by carbon black, rubber and calcium stearate.

Application: Designed for production of pipes used for explosive material, as well as for production of carpets and table cloths where the absence of static electricity charges is necessary.

Information Provided by Kazanorgsintez

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.10 %<= 0.10 %
Carbon Black Loading >= 18.5 %>= 18.5 %
Melt Flow 0.10 - 1.0 g/10 min0.10 - 1.0 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 145 %>= 145 %
Tear Strength Test >= 9.5>= 9.5MPa
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cm
 
Descriptive Properties
AppearanceBlack pellets. Their size in any direction has to be 1.4 to 5 mm.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKAZAN073 / 127392

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.