Applications: Scandia Ceria Stabilized Zirconia is a compound ceramic material composed of scandium oxide (Sc2O3), cerium oxide (CeO2), and zirconium oxide (ZrO2) used as a solid-state electrolyte or cermet anode component in solid oxide fuel cells. Molecular Formula: Sc2O3 / CeO2 / ZrO2 Alfa Chemistry Materials product group: Metal Manufacturer data sheet |
Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |