Bormed™ RE806CF is a random copolymer. The material is specially formulated for medical applications. Applications: Bormed™ RE806CF is recommended for medical packaging. Bormed™ RE806CF contains no slip, antiblock, antistatic additives or nucleating additives.Information provided by Borealis AG |