MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
World Class Technologies Magna Purge® PP 105 Purge Compound
Categories: Polymer; Thermoplastic; Purging Compound

Material Notes: 95% modified PP + 5% chemical compound. FDA compliant components.

Recommended product for injection, blow molding, extrusion and hot runner applications processing within a range of 360°F to 610°F. Eliminates having to stock multi grades of purging compounds recommended by other producers for different resins and processes. Cost effective.

Information provided by World Class Technologies, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 610 °F
Minimum Service Temperature, Air 360 °F
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
World Class Technologies Magna Purge® PP 105 G Purge Compound
TIMCAL TIMREX® PP 25 Natural Flake Graphite
TIMCAL TIMREX® PP 10 Natural Flake Graphite
Elmet-Starck Pure Molybdenum Plate, PP-22-2
BP Amoco Acctuf® 3950 Impact Copolymer Polypropylene

PWORLD990 / 185390

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.