MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
BASF Master Builders Solutions ChemRex® CX-25 Polyurethane Adhesive/Sealant  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: CX-25 is a polyurethane based one-component, moisture curing adhesive/sealant. It provides fast cure, non-sag, excellent adhesion and has elastomeric properties with high strength which can reduce/eliminate mechanical fasteners.

Typical applications of CX-25 include sealing of interior /exterior joints, waterproofing overlap seams, bonding roof bows and floors, bonding or sealing side posts, bonding vehicle trim and side molding, bonging diamond-bead plates, and bonding/sealing compartment doors.

Tack-free time is 35 minutes ± 5 minutes given the ASTM C 679 test method. Sag resistance is excellent given the ASTM C 639 test method. The tear strength is 50 pits ± 5 pits given the ASTM D 1044 test method. Lap shear strength is 160 psi ± 10 psi given the ASTM D 1002 test method. Bond durability on glass, aluminum, and concrete is 12.5 % given the ASTM C 719 test method. No degradation occurs after 3000 hours of testing using the accelerated weathering Atlas 6500 Xenon arc model.

Information provided by ChemRex, Inc.

Product of former ChemRex, Inc. BASF launched the Master Builders Solutions brand on January 15, 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55ASTM C661
Tensile Strength, Ultimate 1.38 - 1.72 MPaASTM D412
Elongation at Break 300 - 400 %ASTM D412
Tear Strength Test 50pit per ASTM D 1044
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °C
Minimum Service Temperature, Air -40.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREX04 / 65563

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.