MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chase Electronic Coatings HumiSeal® 1B73LOC Acrylic Conformal Coating
Categories: Polymer; Thermoset

Material Notes: HumiSeal® 1B73LOC is a low VOC solvent based conformal coating that complies with most North American air quality regulations. HumiSeal® 1B73LOC is a fast drying, single component, acrylic coating intended for printed circuit assemblies. Cured HumiSeal® 1B73LOC fluoresces under UV light for ease of inspection and is easily repaired. HumiSeal® 1B73LOC coating is MIL-I-46058C qualified, IPC-CC-830 and RoHS Directive 2011/65/EU compliant and recognized under UL File Number E105698.

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D1475
Solids Content 26 %26 %± 2%. By weight; Fed-Std-141, Meth. 4044
Volatile Organic Compounds (VOC) Content 92 g/l92 g/l
Viscosity 415 - 475 cP415 - 475 cPFed-Std-141, Meth. 4287
Thickness 25.0 - 75.0 microns0.984 - 2.95 milRecommended coating
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 0.0111 GPa1.61 ksiDMA
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 7.00e+10 ohm7.00e+10 ohmMoisture; MIL-I-46058C
 5.50e+14 ohm5.50e+14 ohmMIL-I-46058C
Dielectric Constant 2.6
@Frequency 1e+6 Hz,
Temperature 25.0 °C
2.6
@Frequency 1e+6 Hz,
Temperature 77.0 °F
ASTM D150-98
Dielectric Breakdown 6300 V6300 VASTM D149
Dissipation Factor 0.010
@Frequency 1e+6 Hz,
Temperature 25.0 °C
0.010
@Frequency 1e+6 Hz,
Temperature 77.0 °F
ASTM D150-98
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.0 µm/m-°C37.2 µin/in-°FTMA
Glass Transition Temp, Tg 42.0 °C108 °FDSC
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 76.0 °C
2.00 hour
@Temperature 169 °F
Option
 1440 min
@Temperature 23.0 °C
24.0 hour
@Temperature 73.4 °F
Option
 10100 min
@Temperature 23.0 °C
168 hour
@Temperature 73.4 °F
Optimum Properties
Tack-Free Time 25.2 min0.420 hourTo handle; Fed-Std-141, Meth. 4061
Shelf Life 24.0 Month
@Temperature 23.0 °C
24.0 Month
@Temperature 73.4 °F
DOM
 
Descriptive Properties
Dielectric Withstand>1500 Vper MIL_I_46058C
Fungus ResistancePassesASTM G21
Thermal Shock-65 to 125°Cper MIL_I_46058C, 50 cycles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAS909 / 239770

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.