Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optimized for low phosphate release, to limit the formation of deposits on electrical contacts. The material has a red-brownish natural color. Key characteristics: - Flame retardant, based on red phosphorous
- Excellent mechanical performance
- UL 94 V0 at 1.5 mm
- UL 94 RTI 110°C at 1.5 mm
- High CTI (600 V)
- Brownish natural color
Information provided by NILIT. |